Εμφάνιση απλής εγγραφής

dc.contributor.author Προμπονάς, Αντώνιος Ε. el
dc.contributor.author Βλησίδης, Δημήτριος Σ. el
dc.date.accessioned 2015-06-13T11:22:36Z
dc.date.available 2015-06-13T11:22:36Z
dc.date.issued 2015-06-13
dc.identifier.uri http://hdl.handle.net/11400/15876
dc.rights Αναφορά Δημιουργού-Μη Εμπορική Χρήση-Όχι Παράγωγα Έργα 3.0 Ηνωμένες Πολιτείες *
dc.rights.uri http://creativecommons.org/licenses/by-nc-nd/3.0/us/ *
dc.source http://www.elsevier.com/ en
dc.subject samples of stone
dc.subject temperature
dc.subject denture construction
dc.subject θερμοκρασία
dc.subject δείγματα της πέτρας
dc.subject κατασκευή οδοντοστοιχιών
dc.title Compressive strength and setting temperatures of mixes with various proportions of plaster to stone en
heal.type journalArticle
heal.classification Medicine
heal.classification Dentistry
heal.classification Ιατρική
heal.classification Οδοντιατρική
heal.classificationURI http://id.loc.gov/authorities/subjects/sh00006614
heal.classificationURI http://skos.um.es/unescothes/C01006
heal.classificationURI **N/A**-Ιατρική
heal.classificationURI **N/A**-Οδοντιατρική
heal.identifier.secondary doi:10.1016/0022-3913(94)90218-6
heal.language en
heal.access campus
heal.publicationDate 1994-07
heal.bibliographicCitation PROMBONAS, A.E. & VLISSIDIS, D.S. (1994). Compressive strength and setting temperatures of mixes with various proportions of plaster to stone. The Journal of Prosthetic Dentistry. [online] 72 (1). p. 95-100. Available from: http://www.elsevier.com/[Accessed 29/03/2005] en
heal.abstract The compressive strength and setting temperature of different proportions of stone to plaster were measured. The water/powder ratio was 40:100 for all combinations. According to the experimental data, samples of stone to plaster in the ratios of 1:1, 1:3, and 1:4 gave an increased compressive strength of 10.3 MPa compared with the strength of plaster alone (8.3 MPa), possibly because of the low amounts of dental stone in the mix. The lowest amount of heat generated (lowest setting temperature) was recorded by the samples made with the ratio of stone/plaster equal to 1:1, which gave a setting temperature of 43 ° C. Thus, the mix made with this ratio of stone to plaster may be the material of choice for filling the upper half of the flask during complete denture construction. en
heal.publisher Elsevier en
heal.journalName The Journal of Prosthetic Dentistry en
heal.journalType non peer-reviewed
heal.fullTextAvailability true


Αρχεία σε αυτό το τεκμήριο

  • Όνομα: 1-s2.0-0022391394902186-main.pdf
    Μέγεθος: 2.290Mb
    Μορφότυπο: PDF

Οι παρακάτω άδειες σχετίζονται με αυτό το τεκμήριο:

Εμφάνιση απλής εγγραφής

Αναφορά Δημιουργού-Μη Εμπορική Χρήση-Όχι Παράγωγα Έργα 3.0 Ηνωμένες Πολιτείες Εκτός από όπου ορίζεται κάτι διαφορετικό, αυτή η άδεια περιγράφεται ως Αναφορά Δημιουργού-Μη Εμπορική Χρήση-Όχι Παράγωγα Έργα 3.0 Ηνωμένες Πολιτείες